      20/09/10 02:25 PM

They do have a process of welding now called plasma welding. And as soon as welded you mayput your finger on it and its just warm. You may do some research on that.Or someone here might know the
information on it.And post for everyone to see. I do have a German Mauser sporter that I bought
from a fellow in or involved with NASA.And 3 side mount scope mount hole had been welded shut
the bead ? or filler is still on the rifle. And except for exactly where the weld filler is.There was no bluing damage at all.??? Whitey

Post Extras Print Post   Remind Me!     Notify Moderator


Entire topic
Subject Posted by Posted on
* Pitting Shikari 14/09/10 05:19 AM
. * * Re: Pitting tinker   14/09/10 12:44 PM
. * * Re: Pitting Shikari   14/09/10 02:22 PM
. * * Re: Pitting whitey   20/09/10 02:25 PM

Extra information
0 registered and 5 anonymous users are browsing this forum.

Moderator:  CptCurl 



Forum Permissions
      You cannot start new topics
      You cannot reply to topics
      HTML is disabled
      UBBCode is enabled

Rating:
Thread views: 1049

Rate this thread

Jump to

Contact Us NitroExpress.com

Powered by UBB.threads™ 6.5.5


Home | Ezine | Forums | Links | Contact


Copyright 2003 to 2011 - all rights reserved