bstrick
(.275 member)
03/05/20 04:31 AM
Re: Steel and Heat Treat for Action

This is what I have found out so far.



Option #2 is to make all parts 36 RC, then Ion Nitride the Falling block.

#1 is to heat treat the block to 42 RC after machining. Ion nitride the contact surfaces only. Main body 36 RC.

Any more input suggestions?