I tend to be lazy but always clean by the day after I've shot the gun, leaving a gun any longer than that is asking for pitting, indeed in very moist areas, even a day's sitting with fouling is asking for trouble. Any pitting you start, will progress & waiting 3 days is really asking for trouble. Of course, this depends on the relative humidity as Dan indicated and which propellent you use.