Itīs a shame that I can't compare loads with most of you people, because I only have used French Tubal powders sofar! I'm considering trying American stuff one of these days...
My 470 load:
106 grains of Tubal 7000, 500gr Sol/RNSP woodleighs, CCI 250 primer and Norma brass (plus energetic crimmping) for 2170 f/sec and nice groupings from my Krieghof.
The chronograph is a must to keep it under control and you even find out that factory ammos from Fed. come out at around 1900 f/sec, Kynock a little better and A-Square around 1.400 from the same double