Thanks for the replies...I smoked the brass tonight and put them in the chamber. Rub marks are about 1.5” from the head. Hopefully the lee sizer can iron out the area enough to chamber a round so I can at least shoot it a few times while I wait on a custom sizing die.

I will probably go with Hornady. Turnaround time with them is 3 to 4 months. I’ve always had good luck with CH4D, I recently had them make a set of 297/250 Rook for me, they are great dies, but turnaround from them was just shy of 2 years.