Lumps get silver solder or brazing alloy, the remainder of the tubes spacers and ribs get a much lower melting soft solder. The lower melting soft solder facilitates adjustments during regulation. Although uncommon among quality guns and rifles, some few makers also use higher melting (hard solders or brazing) on the barrels/ribs. Cheers Tinker |