Rhodes
(.275 member)
27/08/13 05:58 PM
Re: Demiblock , Shoelump or ?

savage458

Silver solder. At least we call it silver solder over here, I believe you guy's call it brazing over there. Heated to 1200F. Here are some links to a couple of older threads with some useful info.

http://forums.nitroexpress.com/showflat....rt=all&vc=1

http://forums.nitroexpress.com/showflat....rt=all&vc=1

If you do a search on alexbeer and ronvella and a few others you will find some very useful info. I'm only a messenger.

I see Alex Beer is active on the forum again so he might chime in with some advice.



Alex if you are reading this do you mind if I ask you a question. I noticed in your previous posts that you used some Bohler products for your actions, mono-blocks and shoe-lumps. EN36A steel and M238 steel. Can you tell us which product you used for each? Also did you machine these out of the hardened steel? or did you buy it annealed, machine it and then harden it?

Thanking you in advance.